High Sensitivity Soft Piezoelectric Ceramics Piezo electric sensor for Hydrophone
Product Description
High Sensitivity Soft Piezoelectric Ceramics Piezo electric sensor for Hydrophone
WuHan Piezohannas Tech.Co .,Ltd is a manufactuer of piezoelectric ceramics ,ultrasonic transducers with strong technology force.With a quality management system and research & development sector,our products are extensively used in most applications.
Piezo Ceramics Disc Description:
- Dimensions: Φ25× 0.2mm
-Material: P-51
-Electrode: electrodes on the both side (customizable )
Fp(Hz)=99200
Kp=0.595
C(pf)=41800
Application: underwater field,hydrophone
Hydrophone Applications:
Piezoelectric material is ideal for making hydrophones. They can change their form and help generate an electrical potential in response to mechanical or external pressure changes. When an electrical voltage is applied to the crystalline ceramic material, the crystalline structure aligns, becomes anisotropic, and carries an electrical charge.
A typical hydrophone has a transducer. This transducer is crucial for converting the incoming sound waves into an electrical voltage. Use of a piezoelectric transducer as an alternative to crystal material is now a popular option in modern-day hydrophone technology.
Standard Size of Piezo Discs:
range of piezo disc to produce:
Diameter: 2mm-120mm
Thickness:0.1mm-30mm
PZT SOFT Material:
"Soft" PZT materials |
The type of soft material |
||||||||
Properties |
PSnN-5 |
PLiS-51 |
PZT-51 |
PZT-52 |
PZT-53 |
PZT-5H |
PZT-5X |
||
Dielectric Constant |
ɛTr3 |
1600 |
2000 |
2200 |
2400 |
2600 |
3200 |
4500 |
|
Coupling factor |
KP |
0.6 |
0.62 |
0.62 |
0.63 |
0.64 |
0.68 |
0.7 |
|
K31 |
0.35 |
0.35 |
0.35 |
0.35 |
0.36 |
0.38 |
0.4 |
||
K33 |
0.68 |
0.7 |
0.68 |
0.7 |
0.7 |
0.76 |
0.77 |
||
Kt |
0.5 |
0.52 |
0.5 |
0.5 |
0.5 |
0.52 |
0.53 |
||
Piezoelectric coefficient |
d31 |
10-12m/v |
-170 |
-197 |
-186 |
-204 |
-227 |
-275 |
-300 |
d33 |
10-12m/v |
400 |
450 |
500 |
520 |
550 |
620 |
750 |
|
g31 |
10-3vm/n |
-12 |
-11.1 |
-9.6 |
-9.8 |
-9.9 |
-9.7 |
-7.5 |
|
g33 |
10-3vm/n |
28 |
25.4 |
25.6 |
24.5 |
23.9 |
22 |
18.8 |
|
Frequency coefficients |
Np |
2000 |
1920 |
1980 |
1980 |
1960 |
1900 |
1960 |
|
N1 |
1466 |
1407 |
1451 |
1451 |
1437 |
1393 |
1437 |
||
N3 |
1825 |
1925 |
1900 |
1900 |
1755 |
1550 |
1800 |
||
Nt |
2100 |
2100 |
2150 |
2150 |
2150 |
2100 |
2200 |
||
Elastic compliance coefficient |
Se11 |
10-12m2/n |
16.6 |
18 |
16.7 |
17 |
17.4 |
18 |
19 |
Machanical quality factor |
Qm |
85 |
80 |
80 |
75 |
75 |
70 |
65 |
|
Dielectric loss factor |
Tg δ |
% |
2 |
2 |
2 |
2 |
2 |
2 |
2 |
Density |
ρ |
g/cm3 |
7.5 |
7.5 |
7.6 |
7.6 |
7.6 |
7.5 |
7.5 |
Curie Temperature |
Tc |
°C |
350 |
345 |
270 |
270 |
270 |
230 |
165 |
Young's modulus |
YE11 |
<109N/m2 |
60 |
56 |
60 |
59 |
57.5 |
56 |
53 |
Poison Ratio |
0.36 |
0.36 |
0.36 |
0.36 |
0.36 |
0.36 |
0.39 |
Test Report of Φ25× 0.2 piezo disc :