1.Dimension:
Size(OD*ID*T) |
50*20*6 |
Capacity(pf) |
2490±10% |
Radial Frequency fr(khz) |
30±5% |
Resonance Impedance zm |
≤15 |
Thick frequency Ft(khz) |
315 |
Coupling Modulus Kr(%) |
≥45 |
Quality Factor(Qm) |
≥800 |
The weight of 5pcs |
1kg |
2. Some Standard Size of PiezoRing
Sizes from 3mm up to 180mm
Thickness from 0.2mm up to 25mm
Choice of metallisation (Silver, Nickel, Gold and others on request)
Wide choice of PZT formulations
Dimension(mm) |
Capacity C(pF) |
Radial Frequency Fr(KHz) |
Resonance Impedance |
Thick Frequency Ft(KHz) |
Coupling Modulus Kr(%) |
Quality Factor Qm |
Φ4×Φ2×2.5 |
60±12.5% |
622± 5% |
<300 |
|||
Φ8xΦ3x1 |
850 ±5% |
188 ±2% |
≤10 |
|||
240±10% |
153±5% |
≤15 |
1020 |
≥45 |
≥800 |
|
Φ12xΦ5x1 |
1170±15% |
130±6% |
≤5.7 |
|||
Φ13.5xΦ7x1.2 |
2000±15% |
1.7MHz |
≤75 |
|||
Φ15xΦ6.5x5 |
0.269nF±10% |
410 ± 2% |
≤15 |
|||
Φ15xΦ7x4 |
316 ± 12.5% |
102 ± 1KHz |
||||
Φ15xΦ8.5x0.7 |
2100±15% |
91 ± 3KHz |
≤12 |
|||
Φ16xΦ7x2.5 |
899±20% |
90± 5% |
<20 |
870 ± 5% |
||
340±10% |
95.8±5% |
≤20 |
512 |
≥45 |
≥800 |
|
Φ18xΦ12x1.2 |
2000±15 |
1.8MHz±5% |
≤75 |
|||
Φ20xΦ10x4 |
480 ± 12.5% |
75 ± 5% |
||||
1000± 12.5% |
50 ± 3KHz |
|||||
Φ22xΦ8.1x6 |
530±20% |
77 ±3 KHz |
≤25 |
|||
Φ24xΦ7x3 |
1500±12.5% |
75± 5% |
||||
Φ24xΦ12x8 |
550±15% |
60 ±3 KHz |
≤25 |
|||
935±10% |
65.5±5% |
≤15 |
512 |
≥45 |
≥800 |
|
Φ28xΦ9x1 |
6650±15% |
2.08MHz±5% |
≤3 |
|||
Φ28xΦ9x6 |
800±15% |
190±5 KHz |
||||
Φ28xΦ9x0.3 |
22000±15% |
6.8MHz±5% |
≤1.5 |
|||
1150±10% |
58.4±5% |
≤15 |
410 |
≥45 |
≥800 |
|
Φ30xΦ10x6 |
990±15% |
59 ±5% |
≤16 |
|||
Φ32xΦ15x5 |
1080±10% |
49.2±5% |
≤15 |
410 |
≥45 |
≥800 |
Φ35xΦ15x5 |
1430±10% |
45.5±5% |
≤15 |
410 |
≥45 |
≥800 |
Φ38xΦ12.7x6.3 |
2000±20% |
44 ±3 KHz |
≤20 |
|||
1750±10% |
43.4±5% |
≤15 |
410 |
≥46 |
≥800 |
|
Φ40×Φ12×5 |
2070±12.5% |
45.9 |
≤15 |
≥46 |
≥800 |
|
Φ40xΦ15x5 |
1970±10% |
42.8±5% |
≤15 |
410 |
≥45 |
≥800 |
Φ40×Φ20×5 |
1700±12.5% |
37.9 |
≤15 |
≥45 |
≥800 |
|
Φ40×Φ17×6 |
1555±12.5% |
40.5 |
≤15 |
≥45 |
≥800 |
|
Φ42xΦ15x5 |
2200±10% |
40±5% |
≤15 |
410 |
≥45 |
≥800 |
Φ42xΦ17x5 |
2110±10% |
38.8±5% |
≤15 |
410 |
≥45 |
≥800 |
Φ45xΦ15x5 |
2580±10% |
38.1±5% |
≤15 |
410 |
≥46 |
≥800 |
Φ50xΦ17x5 |
3160±10% |
34.8±5% |
≤15 |
410 |
≥45 |
≥800 |
Φ50xΦ17x6 |
2430±10% |
34.8±5% |
≤15 |
315 |
≥45 |
≥800 |
Φ50×Φ20×5 |
2700± 12.5% |
33± 2KHz |
||||
2490±12.5% |
33.2 |
≤15 |
≥45 |
≥800 |
||
Φ50×Φ30×13 |
1350±5% |
200±2 KHz |
≤4 |
|||
Φ50×Φ27×6 |
2100±12.5% |
29.3 |
≤15 |
≥45 |
≥800 |
|
1922±12.5% |
25.3 |
≤15 |
≥45 |
≥800 |
||
Φ60×Φ50×2 |
128±10% |
1MHz±5% |
≤10 |
|||
Φ63.5×Φ50.8×12.7 |
1000 |
127khz |
3.Typical value of "Hard" PZT materials performance:
Hard" PZT materials |
|||||||
Properties |
PZT-41 |
PZT-42 |
PZT-43 |
PZT-82 |
PBaS-4 |
||
Dielectric Constant |
ɛTr3 |
1050 |
1250 |
1420 |
1100 |
1900 |
|
Coupling factor |
KP |
0.58 |
0.58 |
0.58 |
0.52 |
0.59 |
|
K31 |
0.32 |
0.33 |
0.34 |
0.3 |
0.34 |
||
K33 |
0.66 |
0.67 |
0.68 |
0.57 |
0.68 |
||
Kt |
0.48 |
0.48 |
0.48 |
0.4 |
0.49 |
||
Piezoelectric coefficient |
d31 |
10-12m/v |
-106 |
-124 |
-138 |
-100 |
-160 |
d33 |
10-12m/v |
260 |
280 |
300 |
240 |
380 |
|
g31 |
10-3vm/n |
-11.4 |
-11.2 |
-11 |
-10.3 |
-9.5 |
|
g33 |
10-3vm/n |
28 |
25.3 |
24 |
25 |
22.6 |
|
Frequency coefficients |
Np |
2280 |
2200 |
2160 |
2280 |
2200 |
|
N1 |
1671 |
1613 |
1583 |
1671 |
1613 |
||
N3 |
1950 |
1900 |
1875 |
1950 |
1850 |
||
Nt |
2250 |
2200 |
2200 |
2300 |
2200 |
||
Elastic compliance coefficient |
Se11 |
10-12m2/n |
11.8 |
12.7 |
13.2 |
11.6 |
13.2 |
Machanical quality factor |
Qm |
1000 |
800 |
600 |
1200 |
2200 |
|
Dielectric loss factor |
Tg δ |
% |
0.3 |
0.4 |
0.5 |
0.3 |
0.5 |
Density |
ρ |
g/cm3 |
7.5 |
7.5 |
7.5 |
7.6 |
7.5 |
Curie Temperature |
Tc |
°C |
320 |
320 |
320 |
310 |
310 |
Young's modulus |
YE11 |
<109N/m3 |
85 |
79 |
76 |
86 |
76 |
Poison Ratio |
0.3 |
0.3 |
0.3 |
0.3 |
0.33 |